1. Corrosion resistance
2. good water resistance
3. Long lasting
4. Specifications can be customized
Color: | |
---|---|
Model Number: | |
Thickness: | |
Width: | |
Length: | |
Package: | |
Standard: | |
Availability: | |
Quantity: | |
geomembrane
zhongloo
geomembrane
Specification
Geomembrane Technical Parameter (GB standard) | |||||||
Spec Properties | GMS0.5 | GMS0.75 | GMS1.0 | GMS1.25 | GMS1.5 | GMS2.0 | GMS2.5 |
Thickness | 0.5mm | 0.75mm | 1.0mm | 1.25mm | 1.5mm | 2.0mm | 2.5mm |
Tensile Properties (each direction) (≥) .yield strength .break strength .yield elongation .break elongation | 7KN/m 10KN/m -- 600% | 10KN/m 15KN/m -- 600% | 13KN/m 20KN/m 11% 600% | 16KN/m 25KN/m 11% 600% | 20KN/m 30KN/m 11% 600% | 26KN/m 40KN/m 11% 600% | 33KN/m 50KN/m 11% 600% |
Density(≥) | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc |
Puncture Restistance (≥) | 120N | 180N | 240N | 300N | 360N | 480N | 600N |
Carbon Black Content | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% |
Carbon black Dispersion | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) |
Tear Resistance (≥) | 56N | 84N | 115N | 140N | 170N | 2255N | 280N |
Oxidative Induction Time(OIT) Standare OIT(≥) | 60min. | 60min. | 60min. | 60min. | 60min. | 60min. | 60min. |
Our Project Cases
customers Can left us a message on our company alibaba account. Our sales staff will be introduced the product details of HDPE Geomembrane and sent product production videos and pictures and inspection certificates to let customers fully understand our professional capabilities in the HDPE geomembrane industry. During the negotiation, we can send samples of geomembrane liner to customers testing. We also can introduce the company’s basic situation, the advantages of our products, and the company’s success stories in fish ponds in recent years. Last but not least, we had also given reasonable suggestions and documentation on how to install, construct and weld in the application of HDPE geomembrane liner in fish pond projects.
Specification
Geomembrane Technical Parameter (GB standard) | |||||||
Spec Properties | GMS0.5 | GMS0.75 | GMS1.0 | GMS1.25 | GMS1.5 | GMS2.0 | GMS2.5 |
Thickness | 0.5mm | 0.75mm | 1.0mm | 1.25mm | 1.5mm | 2.0mm | 2.5mm |
Tensile Properties (each direction) (≥) .yield strength .break strength .yield elongation .break elongation | 7KN/m 10KN/m -- 600% | 10KN/m 15KN/m -- 600% | 13KN/m 20KN/m 11% 600% | 16KN/m 25KN/m 11% 600% | 20KN/m 30KN/m 11% 600% | 26KN/m 40KN/m 11% 600% | 33KN/m 50KN/m 11% 600% |
Density(≥) | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc |
Puncture Restistance (≥) | 120N | 180N | 240N | 300N | 360N | 480N | 600N |
Carbon Black Content | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% |
Carbon black Dispersion | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) |
Tear Resistance (≥) | 56N | 84N | 115N | 140N | 170N | 2255N | 280N |
Oxidative Induction Time(OIT) Standare OIT(≥) | 60min. | 60min. | 60min. | 60min. | 60min. | 60min. | 60min. |
Our Project Cases
customers Can left us a message on our company alibaba account. Our sales staff will be introduced the product details of HDPE Geomembrane and sent product production videos and pictures and inspection certificates to let customers fully understand our professional capabilities in the HDPE geomembrane industry. During the negotiation, we can send samples of geomembrane liner to customers testing. We also can introduce the company’s basic situation, the advantages of our products, and the company’s success stories in fish ponds in recent years. Last but not least, we had also given reasonable suggestions and documentation on how to install, construct and weld in the application of HDPE geomembrane liner in fish pond projects.