This browser does not support the video element.
HDPE smooth geomembrane is produced from high density polyethylene resin by film-blowing process, adding carbon black, antioxidant, anti-aging and UV-resistance component. Now it is the most widely used products for solid waste containment (such as landfill liners), mining and water containment applications.
1. Food grade materials
PE is no poison, no odor, stable in chemistry, it will bring no pollution at all to the plants, aquatic being,dissolvant it holds, completely FOOD GRADE MATERIALS;
2. Seepage control
Seepage control is the core fuction of geomembrane, for fish ponds, waste landfill and mines and so on; LDPE LLDPE 0.5mm 1mm 1.5mm 2mm waterproof membrane dam pond liner HDPE Geomembrane price
3.MOQ
For MOQ of our geomembranes, if the destination port is in China, any quantity is acceptable, such as the warehouse you have in China;
If the destination port is abroad, the MOQ of our geomembrane is at least 3 rolls.
Take the shipping cost into consideration, you are strongly advised to buy in containers.
4.Virgin or recycled materials
As known to all, there are virgin and recycled materials for geomembrane, You could make your choice by your design. LDPE LLDPE 0.5mm 1mm 1.5mm 2mm waterproof membrane dam pond liner HDPE Geomembrane price
If you are not sure about the design, usually in conditions below, you had better use virgin materials:
A. Directly used under the sun, better use the virgin geomembrane;
B. Thickness below 0.5mm(not included), better use virgin geomembrane;
C. Where the recycled could be used, the virgin could always be used;
D. Places or programs that are difficult to maintain, better use virgin materials.
5. Size choice
Thickness: Choose the thickness you need by your design paper; If no design paper, for fish ponds, virgin 0.5mm geomembrane is advised; for landfill, over 1.5mm thick is advised; for biogas pool, 1.0mm virgin on top is advised, the other being 0.75mm thick;
Width: 5.8m wide for 20' container, 8m wide for 40' container, 8m wide at most; Since there is 20cm welding connect, we'd better make it as wide as possilble;
Length: usually 50m or 100m, but almost any length could be customized; Usually within 1000-2000m long at most; LDPE LLDPE 0.5mm 1mm 1.5mm 2mm waterproof membrane dam pond liner HDPE Geomembrane price
6. LifespanLDPE LLDPE 0.5mm 1mm 1.5mm 2mm waterproof membrane dam pond liner HDPE Geomembrane price
Top quality PE could be used over 50 years, when used in bad environment, like too hot, too cold or heavy acid places, the lifespan will be shorter than 50 years;
7.Caculate of quantity
If you know well about caculating the quantity, please ingore this part.
If not, when you caculate the quantity, please do not forget the welding connection 20cm and edge loss 50cm. LDPE LLDPE 0.5mm 1mm 1.5mm 2mm waterproof membrane dam pond liner HDPE Geomembrane price
8.InstallmentLDPE LLDPE 0.5mm 1mm 1.5mm 2mm waterproof membrane dam pond liner HDPE Geomembrane price
Welding machines involved could be supplied, too. If you do not know much about how to weld and install the geomembrane, we will supply free installment and welding instructions and videos, so you only need to arrange other issues.
Specification
0.5mm 0.75mm 1mm Heavy Waterproof HDPE Geomembrane Pond Liner for Fish Shrimp Farm Price
Geomembrane Technical Parameter (GB standard) | |||||||
Spec Properties | GMS0.5 | GMS0.75 | GMS1.0 | GMS1.25 | GMS1.5 | GMS2.0 | GMS2.5 |
Thickness | 0.5mm | 0.75mm | 1.0mm | 1.25mm | 1.5mm | 2.0mm | 2.5mm |
Tensile Properties (each direction) (≥) .yield strength .break strength .yield elongation .break elongation | 7KN/m 10KN/m -- 600% | 10KN/m 15KN/m -- 600% | 13KN/m 20KN/m 11% 600% | 16KN/m 25KN/m 11% 600% | 20KN/m 30KN/m 11% 600% | 26KN/m 40KN/m 11% 600% | 33KN/m 50KN/m 11% 600% |
Density(≥) | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc | 0.940g/cc |
Puncture Restistance (≥) | 120N | 180N | 240N | 300N | 360N | 480N | 600N |
Carbon Black Content | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% | 2.0-3.0% |
Carbon black Dispersion | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) | Noted(1) |
Tear Resistance (≥) | 56N | 84N | 115N | 140N | 170N | 2255N | 280N |
Oxidative Induction Time(OIT) Standare OIT(≥) | 60min. | 60min. | 60min. | 60min. | 60min. | 60min. | 60min. |
Our Project Cases
Packed in woven geotextile and strength belt or PE film Or packed according to customers' requirements such as mark the company Logo (Export standard package)
FAQ:
Q:Can you send samples?
A:Yes,we are very happy to provide you with free samples to check the quality of our products.
Q:Are you a manufacturer or a trading company?
A:Our company located in Hefei,Anhui Province,with are gistered capital of 52 miion yuan.It is a professiona lmanufacturer of geomembrane,geotextile,geogrid and other products.So we have the competitive price with best quality.
Q:Can you produce the product according to customers' requirements?
A:Sure,we are professional manufacturer,OEM and ODM are both welcome.
Q:How long is the delivery time?
A:General within 3-7days after received the deposit
Q:How to control product quality?
A:Our factory adopts lean management,products from the beginning to the end of the production process have strict quality control.All products must be strictly tested before packing and shipping